Description:Jan 30, 2020018332Preparation procedure of composite sintered brick by iron ore tailing, coal gangue powder, sewage sludge and shale. To remove the water content, the brick body was dried at room temperature 20 177 5 176C for 48 h and then put it in the oven at 105 176C for 24 h.